dc.descriptionO aumento da utilização de materiais poliméricos nos diversos setores da indústria, tem resultado em vários problemas ambientas visto que, com esse crescimento demasiado, ocorreu a geração de uma grande quantidade de resíduos poliméricos. Uma alternativa para diminuir esses impactos ambientais, é o reaproveitamento destes materiais, desenvolvendo compósitos poliméricos reciclados com a adição de fibras naturais, como por exemplo a fibra da coroa do abacaxi. No presente trabalho foram desenvolvidos em extrusora duplarrosca, compósitos de polietileno de alta densidade reciclado (PEADr) reforçado com 10, 20, 30 e 40 % em massa de fibra da coroa do abacaxi, seguido do processo de injeção. O efeito da adição das fibras no compósito foi avaliado por meio da morfologia, propriedades mecânicas, térmicas e físicas. Através da microscopia eletrônica de varredura analisou-se a dispersão e adesão das fibras. Constatou-se que o processo de extrusão em duplarrosca ocasionou a distribuição homogênea das fibras na matriz, enquanto que, a interação fibra/matriz apresentou baixa adesão, interferindo nas propriedades mecânicas (resistência à tração, resistência à flexão e resistência ao impacto). A densidade dos compósitos aumentou de forma gradual com o aumento do teor de fibras. A resistência à tração e a resistência ao impacto dos compósitos apresentaram uma diminuição com a adição do teor em massa de fibra. Por outro lado, a resistência a flexão aumentou gradualmente com o aumento do teor de fibras na matriz, até a incorporação de 30 % em massa de fibras. Por meio da análise termogravimétrica, observou-se que as fibras apresentam estabilidade térmica inferior ao polímero. O aumento do teor de fibras também ocasionou a redução da estabilidade térmica do compósito. De forma geral, os resultados demostraram que não ocorreu adesão entre as fibras e a matriz, mesmo com a elevada quantidade de extrativos presentes na superfície das fibras da coroa do abacaxi. O teor de 30% em massa de fibras incorporado ao PEADr mostrou os resultados mais promissores em termos de resistência a flexão, indicando que, as fibras podem contribuir para aumentar a rigidez do compósito. [resumo fornecido pelo autor]pt_BR
dc.description.abstractThe increased use of polymeric materials in various sectors of industry has resulted in several environmental problems, since, with this growth too, there was the generation of a large amount of polymeric waste. An alternative to reduce these environmental impacts is the reuse of these materials, developing recycled polymeric composites with the addition of natural fibers, such as pineapple crown fiber. In the present work, twin screw extruder, recycled high density polyethylene composites (PEADr) reinforced with 10, 20, 30 and 40 % mass of pineapple crown fiber, followed by the injection process, were developed. The effect of fiber addition in composite was evaluated by morphology, mechanical, thermal and physical properties. By scanning electron microscopy, the dispersion and adhering of the fibers were analyzed. It was found that the double screw extrusion process caused the homogeneous distribution of fibers in the matrix, while the fiber/matrix interaction showed low strength, interfering in mechanical properties (tensile strength, bending resistance and impact resistance). The density of composites increased gradually with the increase of the fiber content. The tensile strength and impact resistance of the composites showed a decrease with the addition of the fiber mass content. On the other hand, the bending resistance gradually increased with the increase of the fiber content in the matrix, until the incorporation of 30 % in fiber mass. Through thermogravimetric analysis, it was observed that the fibers have lower thermal stability than the polymer. The increase in fiber content also caused the reduction of the thermal stability of the composite. In general, the results showed that there was no fit between the fibers and the matrix, even with the high amount of extractives present on the surface of the pineapple crown fibers. The 30% mass content of fibers incorporated into the PEADr showed the most promising results in terms of bending resistance indicating that fibers can contribute to increase composite stiffness. [resumo fornecido pelo autor]en
dc.language.isoptpt_BR
dc.subjectPolietilenopt_BR
dc.subjectPolímerospt_BR
dc.titleAvaliação das propriedades mecânicas, térmicas e físicas de compósitos de polietileno de alta densidade reciclado reforçado com fibras das coroa do abacaxipt_BR
dc.typeTCCpt_BR
mtd2-br.advisor.instituationUniversidade de Caxias do Sulpt_BR
mtd2-br.program.nameEngenharia Química - Bachareladopt_BR
mtd2-br.campusCampus Universitário de Caxias do Sulpt_BR


Arquivos deste item

Thumbnail

Este item aparece na(s) seguinte(s) coleção(s)

Mostrar registro simples