dc.descriptionEste trabalho apresentou um estudo sobre a influência da intensidade de pressão e vazão do fluido lubrirrefrigerante no comportamento do processo de retificação cilíndrica externa. Para a análise dos resultados foram mantidos constantes as condições de usinagem e variou-se os valores de pressão e vazão do fluido de corte. Os ensaios foram realizados em duas etapas sendo na primeira com um rebolo convencional de óxido de alumínio, retificando como corpo de prova brocas de aço SAE M2, com dureza média de 62 à 65 HRc (dureza Rockwell). A partir dos resultados obtidos verificou-se que não houveram alterações microestruturais na subsuperfície analisada através de microscopia óptica, ao mesmo tempo que com o aumento dos valores de pressão e vazão do fluido de corte, diminuíram as marcas escurecidas da região afetada superficialmente pelo calor até a vazão de 60 l/min. Para os experimentos de furação da segunda etapa o critério de fim de vida utilizado foi a quantidade de material usinado. O principal mecanismo de desgaste foi a abrasão e o tipo de desgaste mais significativo foi o lascamento. Os esforços axiais obtidos nos ensaios, após análise estatística dos dados através do método de Fisher, demonstrou que não houveram diferenças entre as cinco condições de aplicação do fluído com relação à força de avanço.pt_BR
dc.description.abstractThis work presents a study on the influence of the pressure and flow intensity of the lubricatingfluid on the external cylindrical grinding process. For the analysis results, the machining conditions were maintained constant, varying the values of pressure and flow of the cutting fluid. The tests were conducted in two phases: first with a conventional aluminum oxide grinding wheel, grinding as specimen SAE M2 steel drills, with an average hardness from 62 to 65 HRc (Rockwell hardness). The obtained results show that there were no microstructural alterations on the sub-surface, analyzed through optical microscopy. As the increased values of the pressure and flow fluid rate showed that the darkened marks of superficially affected region decreased when the flow rate is at 60 liters per minute. For the drilling experiments of the second stage the end of life criteria used was the amount of machined material. Abrasion was the main mechanism of wear as chipping being the most significant type of wear. The axial forces on the surveys, after data analysis through Fisher method, it was shown there were no differences among the five circumstances of the application of the fluid regarding the feed force.en
dc.language.isoptpt_BR
dc.subjectBrocas (Ferramentas)pt_BR
dc.subjectUsinagempt_BR
dc.subjectRetificação e polimentopt_BR
dc.subjectLubrificação e lubrificantespt_BR
dc.subjectDrills (Tools)en
dc.subjectMachiningen
dc.subjectGrinding and polishingen
dc.subjectLubrication and lubricantsen
dc.titleInfluência da vazão e pressão do fluído lubrirrefrigerante na afiação de brocas de aço-rápido M2pt_BR
dc.typeDissertaçãopt_BR
mtd2-br.advisor.instituationUniversidade de Caxias do Sulpt_BR
mtd2-br.advisor.latteshttp://lattes.cnpq.br/6194698838218157pt_BR
mtd2-br.author.lattesFERRONATTO, G.pt_BR
mtd2-br.program.nameBacharelado em Engenharia Mecânicapt_BR


Arquivos deste item

Thumbnail

Este item aparece na(s) seguinte(s) coleção(s)

Mostrar registro simples